Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break 69.0 MPa
10000 psi
chs 2.0 in/min; ASTM D638
Tensile Strength, Yield 62.0 MPa
8990 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 132 %
132 %
chs 2.0 in/min; ASTM D638
Flexural Strength 98.5 MPa
14300 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 2.274 GPa
329.8 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 7.48 J/cm

@Thickness 3.17 mm
14.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 67.5 µm/m-°C

@Temperature -40.0 - 33.9 °C
37.5 µin/in-°F

@Temperature -40.0 - 93.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 133 °C
271 °F
0.125";; ASTM D648