Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L4536 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Flexural Strength | 98.6 MPa | 14300 psi | initial |
Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler Product data demonstrates the effect of the Novakup (lamellar quartz surface treated with 0.5% A-1100) filler. A separate entry demonstrates the effect of untreated Novacite filler in thermopla.. |
|||
Flexural Strength | 98.62 MPa | 14300 psi | ASTM D790 |
Lucent Polymers PC-1406 Polycarbonate, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 98.62 MPa | 14300 psi | ASTM D790 |
Lucent Polymers PC-1406FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 98.62 MPa | 14300 psi | ASTM D790 |
Lucent Polymers PC-1410 Polycarbonate, Injection/Extrusion Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 98.62 MPa | 14300 psi | ASTM D790 |
Lucent Polymers PC-1410FD Polycarbonate, FDA Compliant, Injection/Extrusion Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 98.62 MPa | 14300 psi | ASTM D790 |
Lucent Polymers PC-1418 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 98.62 MPa | 14300 psi | ASTM D790 |
Lucent Polymers PC-1418FD Polycarbonate, FDA Compliant, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 98.62 MPa | 14300 psi | ASTM D790 |
Lucent Polymers PC-1425 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 98.62 MPa | 14300 psi | ASTM D790 |
Lucent Polymers PC-1428 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 98.62 MPa | 14300 psi | ASTM D790 |
Lucent Polymers PC-1428FD Polycarbonate, FDA Compliant, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Techmer ES Elastoblend® PA12 CL Availability: North AmericaForms: PelletsAppearance: Clear/TransparentInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Techmer ES HiFill® ABS GF5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive) Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 32.. |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
CPC - Vycom Corzan® CPVC Chlorinated PVC Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-sup.. |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Entec Hyrene® PSCRY 1.5 General Purpose Polystyrene Available in North America Features: Crystal, High Heat Resistance, General Purpose, High Molecular WeightRoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Strength | 98.5 MPa | 14300 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers PC 0614UV UV Stabilized Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 98.5 MPa | 14300 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers PC 2418 R UV UV Stabilized/Mold Release Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |