Material Notes:
Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.Impact modified, very clear, moderate flow.Information provided by Amco Plastic Materials.
Physical Properties Metric English Comments
Melt Flow 2.7 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.7 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.8 MPa
4750 psi
ASTM D638
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Elongation at Break 52 %
52 %
ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Strength 66.9 MPa
9700 psi
ASTM D638
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 6.35 mm,
Temperature 22.8 °C
1.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 98.9 °C
210 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 3.1 %
3.1 %
ASTM D1003
Transmission, Visible 91.6 %
91.6 %
ASTM D1003