A. Schulman LP479-01 High-Density Polyethylene Homopolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman LP479-01 High-Density Polyethylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Melt Index of Compound 0.80 g/10 min
0.80 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Yield 29.3 MPa
4250 psi
2"/min; ASTM D638
Elongation at Break 260 %
260 %
2"/min; ASTM D638
Flexural Stiffness 827 MPa
120000 psi
ASTM D747
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648
Vicat Softening Point 127 °C
261 °F
ASTM D1525