| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded |
| Manufacturer | Diamond and Network Polymers |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Diamond Polymers ABS 6501 Injection Molding Grade, Extra High Impact.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.03 g/cc | 1.03 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
| Melt Flow | 0.50 g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C |
0.50 g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F |
ASTM D1238 |
| 1.7 g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C |
1.7 g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 101 | 101 | ASTM D785 |
| Tensile Strength, Yield | 38.6 MPa | 5600 psi | chs 2 in/min; ASTM D638 |
| Flexural Modulus | 1.881 GPa | 272.8 ksi | tangent; chs 0.05 in/min; ASTM D790 |
| Izod Impact, Notched | 4.00 J/cm <br>@Thickness 3.17 mm,<br> Temperature 23.0 °C |
7.49 ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 106 °C <br>@Load 1.00 kg,<br> Thickness 3.17 mm |
223 °F <br>@Load 2.20 lb,<br> Thickness 0.125 in |
ASTM D1525 |