Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.881 GPa | 272.8 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 6501 Injection Molding Grade, Extra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |