Mechanical Properties Metric English Comments
Flexural Modulus 1.881 GPa
272.8 ksi
tangent; chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 6501 Injection Molding Grade, Extra High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.