Techmer ES HiFill® PA6/6 GF/M15 HS L BK 40/15% Glass/Mineral Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled , Nylon 66, Heat Stabilized
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 GF/M15 HS L BK 40/15% Glass/Mineral Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 15% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 131 MPa
19000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 248 MPa
36000 psi
ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 9.08 J/cm

@Thickness 3.17 mm
17.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.6 µm/m-°C
12.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 246 °C
475 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 232 °C
450 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+14 ohm-cm
8.00e+14 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149