Material Notes:
Master Bond UV15-7DC is a one component, dual cure UV system for high performance bonding, sealing, coating and encapsulation applications. This system features a primary cure utilizing UV light and a secondary cure that requires heating for curing “shadowed out” sections that are not exposed to UV light. The heat required for polymerization is 250-300°F for 15-30 minutes. The UV part of the curing system is most often used for fixturing with the heat curing cycle being added to complete the cure.
Physical Properties Metric English Comments
Viscosity 1500 - 2500 cP

@Temperature 23.0 °C
1500 - 2500 cP

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D >= 70
>= 70
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Descriptive Properties Value Comments
Color Transparent