Polymer Property : Tensile Strength, Yield = 5600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.6 MPa
5600 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Gravi-Tech™ GRV-PS-027-BA-WHT Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Tensile Strength, Yield 38.6 MPa

@Thickness 3.20 mm
5600 psi

@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Pinnacle Polymers 1402 C Clarified Polypropylene Homopolymer Thermoforming Grade
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Tensile Strength, Yield 38.6 MPa
5600 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 38.6 MPa
5600 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM D638
M. Holland Company PP510 Polypropylene Homopolymer
AntistaticGood flowHomopolymerNucleatedGood stiffnessApplications: CapsClosuresDisposable hospital goodsHousehold goods
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM D638
Global MPP-120-C 20% Mica Reinforced Polypropylene
Information provided by Global Polymers Corporation.
Tensile Strength, Yield 38.6 MPa
5600 psi
2 in/min.; ASTM D638
Ineos H12Z-02 Polypropylene Homopolymer, Antistatic and Nucleated
A nucleated and antistated polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications that require superior mold release pro..
Tensile Strength, Yield 38.6 MPa
5600 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® FRA205 ABS
Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM-D638
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade
Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng..
Tensile Strength, Yield 38.6 MPa

@Temperature 23.0 °C
5600 psi

@Temperature 73.4 °F
ASTM D638
Ineos H35Z-00 Polypropylene Homopolymer
This is a high flow rate, nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 C..
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM D638
Techmer ES HiFill FR® ASA FR-2A WT209
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant, Good Toughness and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc.
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM D638
Techmer ES HiFill® PP GF30 TL15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: LubricatedInformation provided by TP Composites..
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM Data
Styron Magnumâ„¢ 9043 ABS, High Gloss Sheet Extrusion Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Yield 38.6 MPa
5600 psi
Longitudinal
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.002" thick)
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet..
Tensile Strength, Yield 38.6 MPa
5600 psi
2" (50mm) per min.; ASTM D638
Formosa Plastics Formolene® 4101N Staple Fiber and Injection Molding Polypropylene
HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101N is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur..
Tensile Strength, Yield 38.6 MPa
5600 psi
2" (50mm) per min.; ASTM D638
Formosa Plastics Formolene® 4142T Injection Molding Polypropylene
Homopolymer with Nucleating, Antistat AdditivesApplications: Appliance, closure and thin wall applications.Formolene 4142T is a low viscosity, highly isotactic polypropylene homopolymer designed pri..
Tensile Strength, Yield 38.6 MPa
5600 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 38.6 MPa
5600 psi
2" (50mm) per min; ASTM D638
Formosa Plastics Formolene® 4143T Homopolymer Polypropylene
Homopolymer for Injection Molded Applications Formolene® 4143T is a highly isotactic polypropylene for use in injection molded applications including cutlery and thin wall components. It contains a..
Tensile Strength, Yield 38.6 MPa
5600 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 38.6 MPa
5600 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 6501 Injection Molding Grade, Extra High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 38.6 MPa
5600 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS VP-11 SHF
Description: High Flow, Flame Retardant ABSInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 38.6 MPa
5600 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA T-110
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 38.6 MPa
5600 psi
chs 0.2 in/min; ASTM D638
Diamond Polymers Centrex® 835 Sheet Extrusion Grade
Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex ..
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM D638
Clariant Renol PA2SP0004 Nylon 6 Alloy
Data provided by Clariant Masterbatches
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM D638
Clariant Renol SB83642580 ASA Polymer
Data provided by Clariant Masterbatches
Tensile Strength, Yield 38.6 MPa
5600 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS VP-11
Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM D638
Aclo Accutech Polypropylene HP0315V Homopolymer High Heat
Approved to GMP.PP.013