Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW200F8 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.2 %
2.2 %
50% RH / 23°C; Similar to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 230 MPa
33400 psi
ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
ISO 527-1/-2
Tensile Modulus 13.0 GPa
1890 ksi
ISO 527-1/-2
Charpy Impact Unnotched 8.50 J/cm²
40.5 ft-lb/in²
ISO 179/1eU
7.50 J/cm²

@Temperature -30.0 °C
35.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eU
1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C
554 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 0.900 mm
HB

@Thickness 0.0354 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Comparative Tracking Index 300 V
300 V
IEC 60112