Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | ASTM E1269 |
Parker Chomerics THERM-A-GAP™ GEL 8010 High Performance Fully Cured Dispensable Gel Description: Parker Chomerics fully cured dispensable GELs eliminate time consuming hand assembly, decreasing installation costs and reducing customer manufacturing and purchasing (logistical) compl.. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | Estimated from similar grades. |
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Specific Heat Capacity | 1.00 - 1.42256 J/g-°C @Temperature 100 - 300 °C |
0.239 - 0.340000 BTU/lb-°F @Temperature 212 - 572 °F |
Average value: 1.21 J/g-°C Grade Count:2 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
Specific Heat Capacity | 1.00 - 1.20 J/g-°C | 0.239 - 0.287 BTU/lb-°F | Average value: 1.13 J/g-°C Grade Count:3 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
Specialty Materials Boron Monofilament Exceptional compression strength. Specialty Materials' Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source.Information prov.. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
Sapco S.SiC Silicon Carbide Information provided by Sapco. |
|||
Specific Heat Capacity | 1.00 - 1.80 J/g-°C | 0.239 - 0.430 BTU/lb-°F | |
Goodfellow Polyvinyl Fluoride (PVF) Film A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v.. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
Cytec Thornel® Graphite Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
Ensinger TECASINT 8001 Polytetrafluoroethylene (PTFE) + Polyimide, 20% (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
Azoty Tarnow™ TARFLEN SG-1 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
Azoty Tarnow™ TARFLEN SG-2 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
Azoty Tarnow™ TARFLEN SM-1 PTFE Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
Azoty Tarnow™ TARFLEN ST PTFE Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | Silicone Property; E1461-01 |
Arlon Thermabond® T-20 NP (99770W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 8 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Ru.. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | Silicone Property; E1461-01 |
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub.. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Specific Heat Capacity | 1.00 J/g-°C | 0.239 BTU/lb-°F | |
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Specific Heat Capacity | 1.00 J/g-°C @Temperature 20.0 °C |
0.239 BTU/lb-°F @Temperature 68.0 °F |
|
Ceradyne Thermo-Sil® Castable TG Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |