Cotronics Resbond™ 7030 High Temperature Ceramic Adhesive, High Strength

Category Ceramic
Manufacturer Cotronics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Resbond™ 7030 High Temperature Ceramic Adhesive, High Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mechanical Properties Metric English Comments
Flexural Strength 10.0 MPa
1450 psi
Compressive Strength 34.5 MPa
5000 psi
Thermal Properties Metric English Comments
CTE, linear 13.5 µm/m-°C

@Temperature 20.0 °C
7.50 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.20 W/m-K
8.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 982 °C
1800 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Dielectric Strength 3.94 kV/mm
100 kV/in