Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 10.0 MPa | 1450 psi | |
Pyrotek B-3A REFRACTORY BOARD Pyrotek B-3A is a high density calcium silicate board specifically designed for demanding applications such as holding furnaces, launder linings and baffle plates. Its high density and superior har.. |
|||
Flexural Strength | 10.0 MPa | 1450 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 10.0 MPa | 1450 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific) LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 10.0 MPa | 1450 psi | Olsen; ASTM D747 |
UBE J3519 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Flexural Strength | 10.0 MPa | 1450 psi | ASTM D790 |
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE. |
|||
Flexural Strength | 10.0 MPa | 1450 psi | Olsen; ASTM D747 |
UBE V206 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Flexural Strength | 10.0 MPa | 1450 psi | |
Cotronics Resbond™ 7030 High Temperature Ceramic Adhesive, High Strength |
|||
Flexural Strength | 10.0 MPa | 1450 psi | |
Du-Co Ceramics DC-187 Magnesium Oxide Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Flexural Strength | 10.0 MPa | 1450 psi | SAE J949 |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Strength | 10.0 MPa @Temperature 65.0 °C |
1450 psi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8255 HS PA6 (Dry) Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and
fle.. |
|||
Flexural Strength | 10.0 MPa @Temperature 120 °C |
1450 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8350 HS PA6 (Dry) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Flexural Strength | 10.0 MPa @Temperature 93.0 °C |
1450 psi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® 8350 HS PA6 (Dry) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Flexural Strength | 10.0 MPa @Temperature 93.0 °C |
1450 psi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® HPN 9350 HS PA6 (Dry) Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res.. |
|||
Flexural Strength | 10.0 - 17.0 MPa @Strain 5.00 % |
1450 - 2470 psi @Strain 5.00 % |
ASTM D790 |
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st.. |
|||
Flexural Strength | 10.0 MPa | 1450 psi | Olsen; ASTM D747 |
UBE V106 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Flexural Strength | >= 10.0 MPa | >= 1450 psi | ISO 178 |
Shandong Guangyin GYBHVNP Polymer Our GYBHVNP products are mainly applied in fuel pipes and brake pipes of automobile and hoses of air conditioner.Information provided by Shandong Guangyin |