Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 1.00e+9 ohm-cm | <= 1.00e+9 ohm-cm | Teil 30; IEC 600093 / VDE 0303 |
Okulen® 2000 PE-UHMW, DryRun OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | Cond. A; IPC 2.5.17.1 |
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Volume Resistivity | >= 1.00e+9 ohm-cm | >= 1.00e+9 ohm-cm | ASTM D257-91 |
NeXolve LaRC™-CP1 Polyimide Transparent polyimide with low moisture uptake and low dielectric constant. Transparent polyimide with low moisture uptake and low dielectric constant. LaRC™ CP1 exhibits the lowest moisture uptak.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 93 |
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Volume Resistivity | 1e+05 - 1.00e+9 ohm-cm | 1e+05 - 1.00e+9 ohm-cm | ASTM D257 |
Haysite SDL® H261 Polyester, Static Dissipative H261 is an advanced composite that combines high temperature resistant and high strength characteristics with static dissipative properties for use as wave and reflow solder pallets. SDL Grade H261.. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS CF5 5% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 5% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF55 HS L 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityAppearance: BlackProce.. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PA6 GF30 AS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: AntistaticAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+10 ohm-cm | 1.00e+9 - 1.00e+10 ohm-cm | Practical Use (Water Absorption 2.5%); ASTM-D257 |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | Practical Use (Water Absorption 2.9%); ASTM-D257 |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | Practical Use (Water Absorption 1.7%); ASTM-D257 |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
Cotronics Resbond™ 7030 High Temperature Ceramic Adhesive, High Strength |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® 2D 25 W 20 HL X black 9992 PA612-I Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Gril.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 60093 |
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | cond; IEC 60093 |
DSM Stanyl® TW271F6J10 (PA46+PTFE)-GF30 30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 60093 |
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 60093 |
DSM Stanyl® TW363 Nylon 46 (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 60093 |
BASF Ultramid® C3U PA66/6 (Conditioned) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia Castable ceramic with high dielectric and physical strength. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 60093 |
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Cond)
(discontinued **) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
Aremco Ceramacast™ 905 Silicon-Ceramic Potting Compound Ceramacast™ 905 is a silicone-bonded, ceramic filled high temperature adhesive and potting compound. |