Material Notes:
Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Used for a variety of processing equipment, particularly to maintain product purity in handling foods, synthetic fibers, and alkalis. Standard product forms are round, flats, pipe, tube, plate, sheet, forging stock, strip, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 462 MPa
67000 psi
Annealed
475 MPa

@Temperature 300 °C
68900 psi

@Temperature 572 °F
Annealed prior to test
Tensile Strength, Yield 148 MPa
21500 psi
Annealed
120 MPa

@Temperature 300 °C
17400 psi

@Temperature 572 °F
Annealed prior to test
Elongation at Break 45 %
45 %
Annealed prior to test.
48 %

@Temperature 300 °C
48 %

@Temperature 572 °F
Annealed prior to test.
Thermal Properties Metric English Comments
CTE, linear 13.3 µm/m-°C

@Temperature 20.0 - 100 °C
7.39 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.456 J/g-°C
0.109 BTU/lb-°F
Thermal Conductivity 70.2 W/m-K
487 BTU-in/hr-ft²-°F
Melting Point 1435 - 1446 °C
2615 - 2635 °F
Solidus 1435 °C
2615 °F
Liquidus 1446 °C
2635 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.15 %
<= 0.15 %
Copper, Cu <= 0.25 %
<= 0.25 %
Iron, Fe <= 0.40 %
<= 0.40 %
Manganese, Mn <= 0.35 %
<= 0.35 %
Nickel, Ni >= 99 %
>= 99 %
Including Cobalt
Silicon, Si <= 0.35 %
<= 0.35 %
Sulfur, S <= 0.010 %
<= 0.010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000960 ohm-cm
0.00000960 ohm-cm
Curie Temperature 360 °C
680 °F