Polymer Property : Flexural Strength = 1450 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 10.0 MPa
1450 psi
Pyrotek B-3A REFRACTORY BOARD
Pyrotek B-3A is a high density calcium silicate board specifically designed for demanding applications such as holding furnaces, launder linings and baffle plates. Its high density and superior har..
Flexural Strength 10.0 MPa
1450 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Flexural Strength 10.0 MPa
1450 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific)
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Flexural Strength 10.0 MPa
1450 psi
Olsen; ASTM D747
UBE J3519 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Flexural Strength 10.0 MPa
1450 psi
ASTM D790
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE.
Flexural Strength 10.0 MPa
1450 psi
Olsen; ASTM D747
UBE V206 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Flexural Strength 10.0 MPa
1450 psi
Cotronics Resbond™ 7030 High Temperature Ceramic Adhesive, High Strength
Flexural Strength 10.0 MPa
1450 psi
Du-Co Ceramics DC-187 Magnesium Oxide
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Flexural Strength 10.0 MPa
1450 psi
SAE J949
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 10.0 MPa

@Temperature 65.0 °C
1450 psi

@Temperature 149 °F
ASTM Test
BASF Ultramid® 8255 HS PA6 (Dry)
Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and fle..
Flexural Strength 10.0 MPa

@Temperature 120 °C
1450 psi

@Temperature 248 °F
ASTM Test
BASF Ultramid® 8350 HS PA6 (Dry)
Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate..
Flexural Strength 10.0 MPa

@Temperature 93.0 °C
1450 psi

@Temperature 199 °F
ASTM Test
BASF Ultramid® 8350 HS PA6 (Dry)
Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate..
Flexural Strength 10.0 MPa

@Temperature 93.0 °C
1450 psi

@Temperature 199 °F
ASTM Test
BASF Ultramid® HPN 9350 HS PA6 (Dry)
Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res..
Flexural Strength 10.0 - 17.0 MPa

@Strain 5.00 %
1450 - 2470 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
Flexural Strength 10.0 MPa
1450 psi
Olsen; ASTM D747
UBE V106 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Flexural Strength >= 10.0 MPa
>= 1450 psi
ISO 178
Shandong Guangyin GYBHVNP Polymer
Our GYBHVNP products are mainly applied in fuel pipes and brake pipes of automobile and hoses of air conditioner.Information provided by Shandong Guangyin