Braskem TI6200Q4 High impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TI6200Q4 High impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Extra high izod impact, superior low temperature drop impact, good paint adhesion. Applications: Suggested uses include toys, video cassettes, compounding. Process: Compounding. This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 66
66
ASTM D785
Tensile Strength 19.7 MPa
2850 psi
2 in/min; ASTM D638
Elongation at Yield 5.5 %
5.5 %
2 in/min; ASTM D638
Flexural Modulus 0.793 GPa
115 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched NB
NB
ASTM D256A
Impact Test 47.5 J

@Temperature -29.0 °C
35.0 ft-lb

@Temperature -20.2 °F
ASTM D3763