Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cossa Polimeri ESTADIENE 1030 V0/Ex Flame Retardant ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTADIENE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cossa Polimeri ESTADIENE 1030 V0/Ex Flame Retardant ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high impact resistance, high gloss, good light resistance, for extrusionInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D 955
Melt Flow 10 g/10 min

@Load 10.0 kg,
Temperature 220 °C
10 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D 638
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D 638
Elongation at Break 6.0 %
6.0 %
ASTM D 638
Flexural Modulus 2.40 GPa
348 ksi
ASTM D 790
Izod Impact, Notched 1.80 J/cm

@Temperature 0.000 °C
3.37 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point 93.0 °C

@Load 5.00 kg
199 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
102 °C

@Load 0.999 kg
216 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Glow Wire Test 960 °C
1760 °F
I.E.C. 695-2-1
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved