Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 2.20 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
4.12 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 2.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
4.12 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87771 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 2.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
4.12 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L4857 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 2.20 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.12 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ISO 180/4A
Polimeri Europa Sinkral® B 432/E ABS Resin
Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific)
Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer
Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific)
Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Europe-Africa-Middle East)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific)
DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r..
Izod Impact, Notched 2.20 J/cm

@Temperature -40.0 °C
4.12 ft-lb/in

@Temperature -40.0 °F
ASTM D256
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)  (Unverified Data**)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific)
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer
Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Europe-Africa-Middle East)
Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.This data was supplied b..
Izod Impact, Notched 2.20 J/cm

@Temperature -30.0 °C
4.12 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East)
Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac..
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 2.1%); ASTM-D256
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned)
Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo.
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTADIENE 1030 V0/Ex Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high impact resistance, high gloss, good light resistance, for extrusionInformation provided by Cossa Polimeri S.r.l.
Copyright © lookpolymers.com All Rights Reserved