Cossa Polimeri ESTABLEND PSA 7600 PC / ASA Blend

Category Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTABLEND PSA
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cossa Polimeri ESTABLEND PSA 7600 PC / ASA Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D 955
Melt Flow 17 g/10 min

@Load 5.00 kg,
Temperature 260 °C
17 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.0 MPa
8410 psi
ASTM D 638
Tensile Strength, Yield 59.0 MPa
8560 psi
ASTM D 638
Elongation at Break >= 50 %
>= 50 %
ASTM D 638
Flexural Modulus 2.25 GPa
326 ksi
ASTM D 790
Izod Impact, Notched 5.60 J/cm

@Temperature 23.0 °C
10.5 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point 132 °C

@Load 5.00 kg
270 °F

@Load 11.0 lb
120°C/hr; ASTM D 1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Glow Wire Test 750 °C
1380 °F
I.E.C. 695-2-12
Users viewing this material also viewed the following: