Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.25 GPa | 326 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EX2079X PC (Europe-Africa-Middle East) Lexan* EX2079X polycarbonate resin, MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retardant, halogen free per DIN VDE 0472 Part 815, mold release, UV stabilized, translu.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LR180 PC (Europe-Africa-Middle East) LR180 is a medium viscosity, non UV, non release containing multipurpose polycarbonate recycle gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Asia Pacific) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C1150E PC+ABS (Asia Pacific) High impact, extrusion grade polycarbonate/ABS alloy. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Flexural Modulus | 2.25 GPa @Thickness 3.17 mm |
326 ksi @Thickness 0.125 in |
|
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.25 GPa @Thickness 3.17 mm |
326 ksi @Thickness 0.125 in |
|
Mitsubishi Iupilon® H2001R 23 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.25 GPa @Thickness 3.17 mm |
326 ksi @Thickness 0.125 in |
|
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.25 GPa @Thickness 3.17 mm |
326 ksi @Thickness 0.125 in |
|
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2mm/min; ASTM D790 |
Kingfa FRHIPS-930 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, 5VA @ 2.6mmNon-DPO, high UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingPrinter, photocopier, fax machineElec.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl V080 PPE+HIPS (Europe-Africa-Middle East) NORYL V080 is an unfilled, flame retardant, high flow material and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | ISO 178 |
Solvay TECHNYL® A 238 Black 21 N PA66, DRY Description: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 238 offers excellent .. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Asia Pacific) PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP D7001IXH PC LNP* THERMOCOMP* D7001IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare ap.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | At 5 mm/min; ISO 178 |
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled Daplen MD206U is a 20% mineral filled polypropylene compound intended for injection molding. MD206U has been developed especially for automotive interior parts that require excellent balance betwee.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | ASTM D790M |
DSM Somos® 14120 Water-resistant resin for stereolithography, White DescriptionDSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to p.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® 300H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.25 - 9.66 GPa @Temperature -40.0 - 150 °C |
326 - 1400 ksi @Temperature -40.0 - 302 °F |
Average value: 4.77 GPa Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | ISO 178 |
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |