Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Yield 33.4 MPa
4840 psi
at elastic yield; ASTM D412
2.65 MPa

@Strain 100 %
384 psi

@Strain 100 %
ASTM D412
5.20 MPa

@Strain 300 %
754 psi

@Strain 300 %
ASTM D412
Elongation at Break 1000 %
1000 %
ASTM D412
Tear Strength 75.4 kN/m
430 pli
Processing Properties Metric English Comments
Melt Temperature 188 - 210 °C
370 - 410 °F
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
Dry Time 2 - 4 hour

@Temperature 104 °C
2 - 4 hour

@Temperature 220 °F
to ensure moisture level is less than 0.02%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.000 - 0.345 MPa
0.000 - 50.0 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm