Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.20 MPa | 754 psi | ASTM D412 |
Precision Polymer Engineering F80X Fluorosilicone Rubber Mid-Blue Fluorosilicone Rubber, 76-85 °IRHD . Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1,.. |
|||
Tensile Strength, Yield | 5.20 MPa | 754 psi | -20% change after 70 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S80D Silicone Rubber Black Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. Formulated to meet UK Ministry of Defence .. |
|||
Tensile Strength, Yield | 5.20 MPa | 754 psi | M100 |
3M Dyneon™ Fluorel™ FT-2320 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 69% F grade terpolymer for difficult ex.. |
|||
Tensile Strength, Yield | 5.20 MPa | 754 psi | |
Dow AFFINITY™ SE 1400 Polyolefin Plastomer AFFINITY® SE 1400 polyolefin plastomer is an ethylene octene resin that offers excellent performance for profile extrusion of thick tubes and good melt strength for low shear blow molding. It has e.. |
|||
Tensile Strength, Yield | 5.20 MPa @Strain 300 % |
754 psi @Strain 300 % |
ASTM D412 |
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 5.20 MPa | 754 psi | |
ACC QM260 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: expanded PU foam, large obje.. |
|||
Tensile Strength, Yield | 5.20 MPa | 754 psi | cured 60 mins @ 100°C |
ACC QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing .. |