Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 75.3 kN/m | 430 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 90453 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 75.4 kN/m | 430 pli | 73°F; ASTM D624 |
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tear Strength | 75.4 kN/m | 430 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
Tear Strength | 75.4 kN/m | 430 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® 18VT80 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 18VT80 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and superior hydrolysis and microbe resistan.. |
|||
Tear Strength | 75.4 kN/m | 430 pli | ASTM D624 |
Huntsman KRYSTALFLEX® PE 505 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Tear Strength | 75.4 kN/m | 430 pli | ASTM D624 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure Liquid, Grey Information provided by ITW Devcon |
|||
Tear Strength | 75.4 kN/m | 430 pli | ASTM D624 |
ITW Devcon Rubber Repair / Castable Urethane Edge & Seal (T-35), Black Information provided by ITW Devcon |
|||
Tear Strength | 75.4 kN/m | 430 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance.. |
|||
Tear Strength | 75.4 kN/m | 430 pli | ASTM D624 |
Multibase Multi-Flex® A 9702 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tear Strength | 75.4 kN/m | 430 pli | |
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Tear Strength | 75.4 kN/m | 430 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 39-020 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerWeatherable GradeApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Extrusion and Moldin.. |