Clariant Renol PA2SP0024 Nylon 6, Flame Retardant, Static Dissipative

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PA2SP0024 Nylon 6, Flame Retardant, Static Dissipative.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Processing Properties Metric English Comments
Melt Temperature 271 - 293 °C
520 - 560 °F
Mold Temperature 65.6 - 79.4 °C
150 - 175 °F
Dry Time 2 - 4 hour

@Temperature 71.1 °C
2 - 4 hour

@Temperature 160 °F
to ensure moisture content is less than 0.2%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm