Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : High Load Melt Index = 12 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 12 g/10 min

@Load 21.6 kg
12 g/10 min

@Load 47.6 lb
ISO 1133
Total Lacqtene® 2001 PBK 44 HDPE pipe  (discontinued **)
LACQTENE® 2001 PBK 44 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2001 PBK 44 is a black compound especially developed for s..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Formosa Plastics Formolene® HL3712 Sheet and Thermoforming HDPE  (discontinued **)
Medium Density Hexene CopolymerApplications: Gas and chemical tank containment liners, pond liners, landfill liners, tunnel liners.Formolene HL3712 has good processability, excellent melt strength, ..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips Marlex® HHM TR-400G Medium density hexene copolymer  (discontinued **)
Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: pond liners, gas and chemical tank containment liners, landfill liner..
High Load Melt Index 12 g/10 min
12 g/10 min
ASTM D1238
Ineos K44-11-128 HDPE
Ineos K44-11-128 is a high molecular weight, high density polyethylene copolymer intended for large part blow molding where the finished product demands good physical performance and low color. Thi..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D 1238
Total 50100.1 HDPE blow molding
Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging. Blow Molding Stock Temperature 370 – 450 ºF Extrusion melt tempera..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Total L425 HDPE Film
Blown film polyethylene grade. Provides excellent bubble stability, exceptional tear strength, high impact and puncture resistance, outstanding clarity and gloss, good stiffness, excellent compatibi..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Formosa Plastics Formolene® HL3812 Film (Hexene) HDPE
Medium Density Polyethylene Formolene® HL3812 is a high molecular weight hexene copolymer resin that is tailored specifically for geomembrane applications. The resin provides an excellent balance o..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
Formosa Plastics Formolene® HP4401 Pipe HDPE
High Density Hexene CopolymerApplications: Potable water, industrial mining, oil and gas gatheringsFormolene HP4401 is a high performance copolymer that is designed for the most demanding requiremen..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer
Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55..
High Load Melt Index 12 g/10 min

@Load 21.6 kg
12 g/10 min

@Load 47.6 lb
ISO 1133
Total Lacqtene® 2001 TBK 46 HDPE pipe  (discontinued **)
LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and ..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
Formosa Plastics Formolene® E927 Film HDPE
High Density Polyethylene High Molecular Weight Bi-Modal Resin For Thin Film Applications Formolene® E927 is a high molecular weight grade of HDPE designed for high drawdown to produce thin films w..
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
Formosa Plastics Formolene® E927ND Film HDPE
High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E927ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi..
Copyright © lookpolymers.com All Rights Reserved