Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.830 GPa | 120 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips HiD® 9062 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM TR-400G Medium density hexene copolymer
(discontinued **) Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: pond liners, gas and chemical tank containment liners, landfill liner.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | 2% Secant-Method 1; ASTM D790 |
Ineos K44-15-123 HDPE Copolymer with Carbon Black Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ CA187 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent paintability, excellent surface appearance, good impact and stiffness balanceApplications:.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ ETA-3131E Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processabilityApplications: molded.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ ETA-3131EUV Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processability, exc.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | 2% Secant; ASTM D790 |
Chevron Phillips Marlex® H525 High Density Polyethylene, Pressure Pipe Grade This high performance PE 4710 HDPE is tailored for demanding pressure pipe applications that require:Good long-term hoop strengthGood resistance to slow crack growthExcellent resistance to slumpAddi.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Ashley Polymers Ashlene® D926 Nylon 12 A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Tipco Tipcolene® MD-TPE MD TPE - Impact Modified Polypropylene Copolymer Compound for Automobile Bumpers High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |