Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplications:Frozen Food Packaging, Heavy Produce Bags, Dry Goods PackagingProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm.Film properties below based on film thickness of 31.8 µm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 0.80 g/10 min
0.80 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
Coefficient of Friction 0.10
0.10
ASTM D1894
Dart Drop 1.30 g/micron
33.0 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Film Tensile Strength at Break, MD 32.0 MPa
4640 psi
ASTM D882
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Optical Properties Metric English Comments
Haze 2.5 %
2.5 %
ASTM D2457
Gloss 80 %
80 %
at 45°. ASTM D 2457
125 %
125 %
at 60°. ASTM D 2457
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 204 °C
399 °F
Copyright © lookpolymers.com All Rights Reserved