Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® TD-9022-D Super Hexene Film Resin Excellent dart impact, High strength, High toughnessApplications: Retail trash bagsAdditives: Process stabilizer, Slip/antiblockFilm properties are typical of blown film extruded at a blowup ratio o.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ISO 5527 |
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ISO 5527 |
Total Finathene® LL 4010 FH 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
Chevron Phillips 1124 Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Processability, Low Gels, Good Sealability, Medium Slip, High AntiblockApplications:Trash Bags and other LinersProcessing Condition.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
Chevron Phillips 2118 Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Impact Strength, Good Heat Seal Characteristics, Good Processability, Low GelsApplications:Trash bags and other linersProcessing Conditions: Extruder 6.3.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
Chevron Phillips 4610 LDPE High Clarity, Bakery Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal CharacteristicsApplic.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin
(discontinued **) Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
Chevron Phillips MarFlex® 1122 Clarity, Liner Grade Film Resin Resin Type: HomopolymerCharacteristics: Good Impact, No slip, No antiblock, Good processability, Good sealabilityApplications:Liners, Trash bagsProcessing Conditions: Extruder 6.35 cm. Screw L/D Ra.. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene .. |
|||
Secant Modulus, MD | 0.160 GPa | 23.2 ksi | ASTM D882 |
DuPont™ Surlyn® 1901 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1901 is a sodium ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultr.. |
|||
Secant Modulus, MD | 0.160 - 0.170 GPa | 23.2 - 24.7 ksi | Average value: 0.162 GPa Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Liner Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and max.. |