Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BEC5012 is a high molecular weight, low flow rate polypropylene block copolymer with very high impact strength. Applications: BEC5012 is recommended for non-pressure pipes and fittings, structured wall pipes and profiles and sheets.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
0.50 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.50 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50mm/min; ISO 527-2
Elongation at Yield 12 %
12 %
50mm/min; ISO 527-2
Tensile Modulus 1.30 GPa
189 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.500 J/cm²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
7.00 J/cm²

@Temperature 23.0 °C
33.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Processing Properties Metric English Comments
Middle Barrel Temperature 190 - 230 °C
374 - 446 °F
cylinder
Die Temperature 200 - 230 °C
392 - 446 °F
Melt Temperature 200 - 230 °C
392 - 446 °F
Head Temperature 200 - 230 °C
392 - 446 °F