Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® TD-9022-D Super Hexene Film Resin Excellent dart impact, High strength, High toughnessApplications: Retail trash bagsAdditives: Process stabilizer, Slip/antiblockFilm properties are typical of blown film extruded at a blowup ratio o.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin Film Properties. Features: Exceptional toughness, high strength with thin films.Applications: Thin films, premium trash bags, ice bags.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin Film Properties. Features: High strength and toughness, low gel count.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin
(discontinued **) Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
Huntsman PE1205 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1905F Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE, LLDPEContains 1500 ppm slip agent and 2600 ppm antiblocking agentRecommended Applications:General purpose bagVeg.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1905FA Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | 1%, Flexural; ASTM D882 |
Braskem Flexus® 7200 LLDPE Cast Film Extrusion Description: Braskem Flexus7200 is a Linear Low Density Polyethylene, metallocene ethylene-hexene copolymer, produced by gas fase process. It was specially designed to provide outstanding processing.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
Huntsman PE1203 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin
(discontinued **) Film Properties. Features: High strength and toughness, low gel count, intended for narrow die gaps.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.190 GPa | 27.6 ksi | ASTM D882 |
Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |