Mechanical Properties Metric English Comments
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE
Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b..
Secant Modulus, MD 0.160 GPa
23.2 ksi
at 1%; ASTM D882
NOVA Chemicals Novapol® TD-9022-D Super Hexene Film Resin
Excellent dart impact, High strength, High toughnessApplications: Retail trash bagsAdditives: Process stabilizer, Slip/antiblockFilm properties are typical of blown film extruded at a blowup ratio o..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ISO 5527
Total Finathene® LL 4010 FE 18 LLDPE film  (discontinued **)
Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ISO 5527
Total Finathene® LL 4010 FH 18 LLDPE film  (discontinued **)
Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
Chevron Phillips 1124 Liner Grade Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Processability, Low Gels, Good Sealability, Medium Slip, High AntiblockApplications:Trash Bags and other LinersProcessing Condition..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
Chevron Phillips 2118 Liner Grade Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: High Impact Strength, Good Heat Seal Characteristics, Good Processability, Low GelsApplications:Trash bags and other linersProcessing Conditions: Extruder 6.3..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
Chevron Phillips 4610 LDPE High Clarity, Bakery Packaging Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal CharacteristicsApplic..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin  (discontinued **)
Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating  (discontinued **)
Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
Chevron Phillips MarFlex® 1122 Clarity, Liner Grade Film Resin
Resin Type: HomopolymerCharacteristics: Good Impact, No slip, No antiblock, Good processability, Good sealabilityApplications:Liners, Trash bagsProcessing Conditions: Extruder 6.35 cm. Screw L/D Ra..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging
Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene ..
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
DuPont™ Surlyn® 1901 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1901 is a sodium ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultr..
Secant Modulus, MD 0.160 - 0.170 GPa
23.2 - 24.7 ksi
Average value: 0.162 GPa Grade Count:4
Overview of materials for Low Density Polyethylene (LDPE), Liner Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and max..