Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips 2118 Liner Grade Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Liner Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 2118 Liner Grade Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: High Impact Strength, Good Heat Seal Characteristics, Good Processability, Low GelsApplications:Trash bags and other linersProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0762 cm. Blow-Up Ratio 2:1.Film properties below based on film thickness of 31.8 µm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.160 GPa
23.2 ksi
ASTM D882
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Coefficient of Friction 0.50
0.50
ASTM D1894
Dart Drop 2.20 g/micron
55.9 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 11 %
11 %
ASTM D2457
Gloss 54 %
54 %
at 45°. ASTM D 2457
75 %
75 %
at 60°. ASTM D 2457
Processing Properties Metric English Comments
Melt Temperature 204 °C
399 °F