Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 2.20 g/micron | 55.9 g/mil | F<sub>50</sub>, ASTM D1709/A |
NOVA Chemicals Novapol® 20% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Dart Drop | 2.20 g/micron | 55.9 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips 2118 Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Impact Strength, Good Heat Seal Characteristics, Good Processability, Low GelsApplications:Trash bags and other linersProcessing Conditions: Extruder 6.3.. |
|||
Dart Drop | 2.20 - 3.30 g/micron | 55.9 - 83.8 g/mil | Average value: 2.78 g/micron Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Liner Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and max.. |