Mechanical Properties Metric English Comments
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin
Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin
Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips 1124 Liner Grade Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Processability, Low Gels, Good Sealability, Medium Slip, High AntiblockApplications:Trash Bags and other LinersProcessing Condition..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips 2118 Liner Grade Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: High Impact Strength, Good Heat Seal Characteristics, Good Processability, Low GelsApplications:Trash bags and other linersProcessing Conditions: Extruder 6.3..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips 4522 LDPE Shrink and Heavy Duty Packaging Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Tensile Strength, Excellent Impact Strength, Very Good Tear Resistance, Very Good Abrasion Resistance, No Slip, No AntiblockApplications:Pallet Shri..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips 5622 LDPE Shrink and Heavy Duty Packaging Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Tensile and Impact Strength, Very Good Abrasion and Tear Resistance, Excellent Retention of Properties after Aging, Wide Range of Shrinkage Characte..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips 5625 LDPE Case Shrink and Bundling Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Superior Impact Strength, Good Abrasion and Tear Resistance, Good Sealing Properties, No Slip, High Antiblock, Easy Openability, Medium Coefficient of Frictio..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips 5658 LDPE Shrink and Bundling Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Abrasion and Tear Resistance, Good Sealing Properties, No Slip, Medium Antiblock, Easy OpenabilityApplications:Shrink Wrap, Bundlin..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips MarFlex® 1122 Clarity, Liner Grade Film Resin
Resin Type: HomopolymerCharacteristics: Good Impact, No slip, No antiblock, Good processability, Good sealabilityApplications:Liners, Trash bagsProcessing Conditions: Extruder 6.35 cm. Screw L/D Ra..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips MarFlex® 5613 LDPE Shrink and Heavy Duty Packaging Film Resin
Resin Type: HomopolymerCharacteristics: Excellent Tensile Strength and Impact Strength, Very Good Abrasion Resistance and Tear Resistance, No Slip, High Antiblock, Medium Coefficient of Friction, Ea..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips MarFlex® 5619 LDPE Shrink and Heavy Duty Packaging Film Resin
Resin Type: HomopolymerCharacteristics: Excellent Tensile and Impact Strength, Good Abrasion and Tear Resistance, Good Resistance to Blocking, Wide Range of Shrinkage Characteristics, Low Slip, Low ..
Secant Modulus, TD 0.180 GPa
26.1 ksi
2% Secant Modulus; ASTM-D882
Braskem TX9003 LDPE Blown Film Extrusion Polyethylene
TX9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance, good optical properties, and high stiffness. These characteristics provide, in some applications, down gaug..
Secant Modulus, TD 0.180 - 0.200 GPa
26.1 - 29.0 ksi
Average value: 0.185 GPa Grade Count:4
Overview of materials for Low Density Polyethylene (LDPE), Liner Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and max..
Secant Modulus, TD 0.180 GPa
26.1 ksi
ASTM D882
Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Secant Modulus, TD 0.180 GPa
26.1 ksi
2% Secant Modulus; ASTM-D882
Braskem TS9003 LDPE Blown Film Extrusion Polyethylene
TS9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance along with good optical properties and high stiffness. These characteristics ensure the production of packag..