Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic FV30G25 POM, 25% Glass Fiber

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic FV30G25 POM, 25% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.015 cm/cm
0.0050 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 82
82
ASTM D785
Tensile Strength, Yield 70.6 MPa
10200 psi
ASTM D638
Flexural Yield Strength 191 MPa
27700 psi
ASTM D790
Izod Impact, Notched 0.392 J/cm
0.735 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 164 °C
327 °F
ASTM D648
Flammability, UL94 HB
HB