Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Formax 609 Acetal, Medium Flow

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Chem Polymer
Trade Name Formax
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Formax 609 Acetal, Medium Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 9 melt flow index, injection molding grade copolymer acetal.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Melt Flow 9.0 g/10 min
9.0 g/10 min
MFI condition not specified
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Yield Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 190 °C
374 °F
Copyright © lookpolymers.com All Rights Reserved