Material Notes:
A 25% glass sphere reinforced nylon 66 offering a balance of rigidity, dimensional stability and surface appearance.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 138 MPa
20000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 6.20 GPa
899 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 282 °C
540 °F