Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 193 MPa | 28000 psi | ASTM D790 |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/30/TF/13/SI/2 Polycarbonate, 30% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/30/TF/15 Polycarbonate, 30% Carbon Fiber Reinforced, PTFE Lubed Carbon Fiber Reinforced, PTFE Lubricated |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | ASTM D790 |
Techmer ES Plastiblend® PBT/ABS GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/20 Polycarbonate, 20% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | ASTM D790 |
Techmer ES HiFill FR® PET GF30 FR X 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | Flexural elongation is 1%; ASTM D790 |
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent.. |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | ASTM D790 |
Clariant Renol 66G33 2% Moly Nylon 66, 33% Glass Fiber Reinforced, 2% Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | ASTM D790 |
Clariant Renol 66G33HSL Nylon 66, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | ASTM D790 |
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Flexural Yield Strength | 193 MPa | 28000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM AR9100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |