California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy

Category Metal , Ferrous Metal , Superalloy , Iron Base
Manufacturer California Fine Wire
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.28 g/cc
0.299 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 552 MPa
80000 psi
Annealed
689 MPa
100000 psi
Stress relieved
862 MPa
125000 psi
Hard
Tensile Strength, Yield 345 MPa
50000 psi
Annealed
483 MPa
70000 psi
Stress relieved
689 MPa
100000 psi
Hard
Thermal Properties Metric English Comments
Thermal Conductivity 10.28 W/m-K
71.34 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Iron, Fe 57 - 59 %
57 - 59 %
Core, as balance
Nickel, Ni 41 - 43 %
41 - 43 %
Core
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000964 ohm-cm
0.00000964 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02