Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.28 g/cc | 0.299 lb/in³ | P/M (97%), 8.52 g/cc theoretical. |
Kennametal Stellite Stellite® 12 PM with P/M Processing Applications: include vane plugs, fuel metering pins, spacer bushings, ball blanks (bearings), race blanks (bearings), diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wea.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
MarkeTech PWO (Lead tungstate, PbWO4) Scintillator Crystal Lead tungstate PbWO4 (PWO) is a new "heavy" highly efficient and "fast" scintillator for high energy physics. It has the shortest radiation length and Moliere radius among the known scintillators, s.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 Hard, 1.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 MH10, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 MH12, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 MH8, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H925 (H925) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.7Formability Ratio (bad Way).. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard, 1.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard, 2.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 MH2, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Special Metals INCONEL® Alloy X-750 A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Crucible Steel PEERLESS A Tool Steel, AISI H21 Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee.. |
|||
Density | 8.28 g/cc @Temperature 199 °C |
0.299 lb/in³ @Temperature 390 °F |
|
Bohler-Uddeholm BeCu Alloy 172 Mold Material Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Carpenter Pyromet® CTX-3 Superalloy, Heat Treated Data provided by Carpenter Technology Corporation.Pyromet® alloy CTX-3 is a high strength, precipitation hardenable superalloy which exhibits a low CTE over a broad temperature range. This alloy a.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Carpenter Pyromet® CTX-3 Superalloy, Heat Treatment for Brazing Cycles over 982°C Data provided by Carpenter Technology Corporation.Pyromet® alloy CTX-3 is a high strength, precipitation hardenable superalloy which exhibits a low CTE over a broad temperature range. This alloy a.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Alloy Wire International RW 122 Hot Cutting Wire - High Strength Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Wall Colmonoy COLMONOY® 4 PTA - Nickel-Base Hard Surfacing Alloy With Chromium Boride Description: Optimized Colmonoy 4 formulation. Designed for PTA Application.Applications: For plasma transferred arc (PTA) application. Information provided by Wall Colmonoy Corporation. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a.. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H1050 (H1050) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Density | 8.28 g/cc | 0.299 lb/in³ | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H775 (H775) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |