Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 862 MPa | 125000 psi | Hard |
California Fine Wire Alloy 20-245 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireInsulatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 862 MPa | 125000 psi | Hard |
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 862 MPa | 125000 psi | Hard |
California Fine Wire Nickel 271 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 862 MPa | 125000 psi | Hard |
California Fine Wire Nickel 272 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |