Polymer Property : Thermal Conductivity = 71.34 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 10.28 W/m-K
71.34 BTU-in/hr-ft²-°F
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy
All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.