Material Notes:
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.Information provided by the manufacturer, Brueggemann Chemical.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 79
79
ISO 868
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ISO 527
Elongation at Break 40 %
40 %
ISO 527
Modulus of Elasticity 2.445 GPa
354.6 ksi
ISO 527
Flexural Modulus 2.485 GPa
360.4 ksi
ISO 178
Shear Modulus 1.00 GPa
145 ksi
torsional
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180, Brittle break
7.00 kJ/m²

@Temperature -40.0 °C
3.33 ft-lb/in²

@Temperature -40.0 °F
Brittle break; ISO 180
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
DIN 53453, Brittle break
0.600 J/cm²

@Temperature -40.0 °C
2.86 ft-lb/in²

@Temperature -40.0 °F
Brittle break; DIN 53453
Thermal Properties Metric English Comments
Melting Point 214 °C
417 °F
DSC
Users viewing this material also viewed the following: