Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 214 °C | 417 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Melting Point | 214 °C | 417 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® BKV 215 W1 902176 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, weather-stabilized |
|||
Melting Point | 214 - 275 °C | 417 - 527 °F | |
Johnson Matthey LM10A Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 214 °C | 417 °F | DSC |
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified Notes: Very high impact and elongation, low flexural modulus material for tubing and wire jacketing applications requiring a soft, flexible product; FMVSS Flammability: Passes, FMVSS 302Processing M.. |
|||
Melting Point | <= 214 °C | <= 417 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escor™ 5000 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5000 is primarily intended for extrusion coating, coextrusion coating, extrusion lamination. Very good adhesion to polar substrates, aluminum foil, metalized films, papers.. |
|||
Melting Point | 214 °C | 417 °F | DSC |
DSM Fibre Intermediates Nyrim® 1500 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Melting Point | 214 °C | 417 °F | DSC |
DSM Fibre Intermediates Nyrim® 1500 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Melting Point | 214 °C | 417 °F | DSC |
DSM Fibre Intermediates Nyrim® 4000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Melting Point | 214 °C | 417 °F | DSC |
DSM Fibre Intermediates Nyrim® 4000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Melting Point | <= 214 °C | <= 417 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade) Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East.. |
|||
Melting Point | 214 °C | 417 °F | |
Brueggemann Chemical Nyrim® 1000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Melting Point | 214 °C | 417 °F | DSC |
Brueggemann Chemical Nyrim® 1000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Melting Point | 214 °C | 417 °F | ASTM D3418 |
Ashley Polymers Ashlene® 830SMS Nylon 6, MoS2 Filled Basic Nylon 6, medium viscosity, lubricated with Molybdenum Disulfide.Data provided by the manufacturer |
|||
Melting Point | 214 °C | 417 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EB464-01 TPC-ET Antisqueak Blow Molding Grade |
|||
Melting Point | 214 - 223 °C | 417 - 433 °F | Average value: 220 °C Grade Count:22 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |