Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.445 GPa | 354.6 ksi | ISO 527 |
Brueggemann Chemical Nyrim® 1000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |