Material Notes:
Injected lids and caps; Large flat surface injected pieces.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.915 g/cc
0.915 g/cc
ASTM D1505/D792
ESCR 10% Igepal® 15 hour

@Temperature 50.0 °C
15 hour

@Temperature 122 °F
h/50%f; compression molded 2 mm notched-plaques; ASTM D1683
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 39
39
ASTM D2240
Tensile Strength at Break 8.00 MPa
1160 psi
ASTM D638
Tensile Strength, Yield 8.00 MPa
1160 psi
ASTM D638
Flexural Modulus, 1% Secant 450 MPa
65300 psi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 79.0 °C
174 °F
ASTM D1525