Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem CX7020 LDPE Cast Film Extrusion Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem CX7020 LDPE Cast Film Extrusion Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CX7020 is a low-density polyethylene (LDPE) with excellent processability and low gel content. Those features allow for production of thin and highly uniform films. This product is identified as PE 113 according to ASTM D-4976-04a standard specification. It does not contain additives. Its applications include: smooth or embossed films for diapers, disposable sheets, etc.; films for lamination; injection-blow molding; and foamed applications. Recommended processing conditions for film extrusion are about 145 - 190 ºC.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM-D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 350 %
350 %
ASTM-D882
Film Elongation at Break, TD 650 %
650 %
ASTM-D882
Secant Modulus, MD 0.130 GPa
18.9 ksi
2% Secant Modulus; ASTM-D882
Secant Modulus, TD 0.140 GPa
20.3 ksi
2% Secant Modulus; ASTM-D882
Elmendorf Tear Strength MD 410 g
410 g
ASTM-D1922
Elmendorf Tear Strength TD 280 g
280 g
ASTM-D1922
Elmendorf Tear Strength, MD 8.20 g/micron
208 g/mil
ASTM-D1922
Elmendorf Tear Strength, TD 5.60 g/micron
142 g/mil
ASTM-D1922
Dart Drop 2.40 g/micron
61.0 g/mil
ASTM-D1709
Dart Drop Test 120 g
0.265 lb
ASTM-D1709
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM-D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 7.5 %
7.5 %
ASTM-D1003
Gloss 65 %
65 %
Angle 45°; ASTM-D2457
100 %
100 %
Angle 60°; ASTM-D2457
Processing Properties Metric English Comments
Die Opening 0.100 cm
0.0394 in
Cast Film Extrusion
Blow-up Ratio (BUR) 2.0 - 3.0
2.0 - 3.0
Cast Film Extrusion
Descriptive Properties Value Comments
Mass Temperature (°C) 190
Cast Film Extrusion
Temperature Profile (°C) 145-190
Cast Film Extrusion
Copyright © lookpolymers.com All Rights Reserved