Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.140 GPa | 20.3 ksi | ASTM D882 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process.. |
|||
Secant Modulus, TD | 0.140 GPa | 20.3 ksi | ASTM D882 |
Eastman 5220 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good bubble stability, Medium coefficient of friction, Excellent low temperature properties, Good heat seal characteristicsApplica.. |
|||
Secant Modulus, TD | 0.140 GPa | 20.3 ksi | ASTM D882 |
Eastman 5222 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good low temperature properties, Good heat seal characteristics, High slip, High antiblock, Good optical propertiesApplications:Ic.. |
|||
Secant Modulus, TD | 0.140 GPa | 20.3 ksi | ASTM D882 |
Eastman 5223 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good heat seal characteristics, High antiblock, No Slip, Good processability. Slip 0 ppm. Antiblock 5000 ppm.Applications:Ice ba.. |
|||
Secant Modulus, TD | 0.140 GPa | 20.3 ksi | ASTM D882 |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Secant Modulus, TD | 0.140 GPa | 20.3 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem CX7020 LDPE Cast Film Extrusion Polyethylene CX7020 is a low-density polyethylene (LDPE) with excellent processability and low gel content. Those features allow for production of thin and highly uniform films. This product is identified as PE .. |
|||
Secant Modulus, TD | 0.140 GPa | 20.3 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness.. |